Aaj ki post  mold ke baare me hai. Ummeed hai apko pasand aaayegi lekin isse pahle aapse request hai ki mere is blog ko aap share jaroor kare aur hamare youtube channel @ezyplast ko subscribe kare .dosto hum instagram pe bhi baahut achchi achchi post late hai aap hume waha bhi follow kariye.

Dosto mold aur kuch nhi bas ek tool hai jisme plastic melt material ko  inject karte hai jisse melt mold me bane hue impression  ka shape leta hai aur product form karta hai .

Iske do part hote hai jinhe core aur cavity bolte hai

Injection nolding machine me fux plate aur moving plate hoti hai

Cavity half ko fix plate me align karte hai aur core plate ko moving plate me allign krte hai 

Dosto cavity plate me  locating ring hoti hai jisse machine aur mold ko properly allignment milta hai is ring ko machine ki ring me is tarah se fasate hai ki machine ka nozzle mold ke centre matlab sprue bush pr hit krta. 

Mold basically 3 type k hote hai

Split mold

2 plate mold

3 plate mold




Comments

Popular posts from this blog

What is suck back in injection molding

 Good morning dosto Suck back , Naam se hi lag rha hai ki koi cheez suck ho rhi hai yani kheechi ja rhi hai . Suck back ka matlab hua peeche ki taraf kheechna  .  Actually jab plastic melt material mold me inject ho jata hai aur injection ke baad holding  complete ho jati hai tab part cooling zone me jata hai aur isi waqt refilling bhi sath sath hoti rhti hai refilling poori hone k baad screw straight direction me back hota hai utne mm jitna set kiya jata hai. Alag alag material k liye alag alag value me set krte hai suck back  Suck back dene se drooling ki problem ko solve kiya jata hai aur sath hi sath   silver bhi troubleshoot hota hai .suck back dene se material me threading generate nhi hoti hai nozzle se  

Types of plastic

Plastic 2 prakar ke hote hai 1 thermoplastic 2 thermosetting plastic Wo plastic jo ek baar heat dene k baad   soft ho jate hai aur easily doosrey article me convert ho jate hai .isme na unki physical property change hoti hai n chemical property change hoti bus sirf physical look change ho jata hai Jabki thermosetting plastic me  agar ek baar kisi article ko heat kiya to fir se wo dobara nhi change nhi hoga aur material degrade ho jaega aur dirty si smell aane lagti hai for example aap cooker k utensil hi lelo .isliye thermoplastics achche hote hai kyuki wo recyclable hote hai . Unse koi bahut jyada environment ka khatra bhi nhi hai . #injection molding #plastic #indiaplast #ezyplast #whatisplastic #typesofplastic #plastasia #polymer

What is l/d ratio

L/d ratio👉 Yah screw ki flight length aur outside diameter Ka anupat Hota Hai jyadatar yah anupat 20:1 hota hai aur ya 18:1 se 24 * 1 Tak hota hai dharmon set material Mein yah anupat 12:1 se 16 is Tu Van tak rahata hai Jyada Se Jyada share hit generate Hoti Hai plastic Mein Bina Jale Hue Jitna Jyada mixing hoti hai utna hi h*** genus melt hota hai Jitna Jyada residence time hota hai plastic ka barrel mein aur LCM Jyada hoga to kam cycle time mein Bade shots nikal Lete Hain. To yah To Kuchh definition Thi doston ab main aapko Aasan bhasha mein samjhata hun ki l y Di ratio Hota kya hai dekhiae jo screw ki lambai hoti hai usko Ham bolate Hain flight length theek Hai Doston Kyunki yah flight Jahan se start hoti hai aur jahan tak flight ka end hota hai rinklanjar wale part Ko Chhod Karke is group mein vah lambai kahlati hai flight length aur jo nominal diameter hota hai is group ka usko Ham outside Tak napte Hain usko Ham bolate Hain out side diameter ine donon ka hi jo ratio Hota Hai vah...