Skip to main content

Injection molding Defect 7 ~shrinkage

 ðŸ‘‹ðŸ‘‹ good morning doston kaise hain aap log ummid hai aap log acche Honge injection molding mein ham log aage badhate hain aur aaj Jaisa ki aapko pata hai ki defective ki series padhte Hue Chale a Rahe Hain To usmein Ham injection molding ke defect shringage ke bare mein padhenge Aaj how Tu remove syncase defect ine injection moulding ka matlab Hindi mein hota hai sikud Jana sikudna Koi chij sikud gai hai koi tarike se Thandi Nahin Ho paati Hai tab vah sikud Jaati Hai shring Ho Jaati Hai To usko kya chahie usko chahie time kaun sa time chahie usko chahie Thanda hone ka time koi chij hited hai per vah theek se uske andar Jo heat hai vah out Nahin Ho Pai Hai uski body se uski sarface se to Vahi kya karti hai usko contract kar deti hai use chij ko fault Ko To Hamen kya karna hai yane ki Sanket defect ko remove karna hai part se yani ki jo heat hai contract ho rahi hai party mein usko Hamen kya karna hai usko exhaust kar dena hai Bahar ko nikal dena hai aur usko kaise karenge usko ham cooling Lekar ke I jyadatar Karte Hain To Chaliye Shuru Karte Hain part ka sikudna hi Sanket kahlata Hai part Mein holes Ho Jaate Hain Iske Kai reasons Hai Jis per Ham thoda sa discuss karte hain Agar ring plunger is group ke andar hota hai ring pleasure Agar vah damage ho jata hai ya usmein metal fans Gaya Hai To part theek se pack Nahin Ho Pata Hai Kisi bhi Tarah Ki catching a lock ya part catching a core catching Agar a rahi hai mood mein to usko jaldi se jaldi polish karvana chahie Kyunki agar aisa nahin kiya Gaya to part Mein catching ki vajah se Sanket ka Aana lagbhag possible hai main Dekha Jaaye to cooling lines per nirbhar Hoti Hai yah Jahan part ka koi area ekadam se garm ho jata hai yah line block Ho Jaati Hai water flow Sahi Nahin Hota Hai to vahan calling samasya Ho Jaati Hai hot runner Ka Maine fold Mein leakage hone per sankir Jata Hai Aur Ka jo maine folder hai agar usmein koi leakage Ho Gaya to kya hoga Singh ke to aaega Kyunki material jo hai vah likhkar Jaega aur part Puri tarike se Bhar Nahin payega to use Tarah Se FIR engage a jata hai agar mold ke gate ki design proper Nahin Hai to engage aaega Yahan per bhi Gate ki design ke bare mein baat ki ja rahi hai iska bhi shringage mein bahut bada roll hota hai leakage mein agar Dekhen ho sakta hai diesel Lo Jal se bhi leakage ho sakti hai ya FIR nojal ke size se related problem ho sakti hai ya Kuchh Bhi problem ho sakti hai related temperature mein bhi problem ho sakti hai yah to bahut hi kam ho sakta hai ya FIR bahut hi jyada ho sakta hai aur holding pressure Agar Dekha Jaaye to jyada hai ya kam hai kam set Karoge To aaega hi sath mein short moulding ki problem bhi Aaegi finger Marg problem bhi aaega isliye short size ko utna Jarur Den itne se part Hamara ban jata hai holding time Kam Nahin Hai To Kya Karna chahie holding time Kam Nahin Hai To aap kya kar sakte hain holding time ko Badha sakte hain aap injection speed injection Agar kam hai to aap kya kar sakte ho Badhai badhaie aur part sahi ho jaega Is Tarah Se Humne Aaj shringage ko padha doston tasvir mein problem jo hai vah cooling ki problem hoti hai jyadatar ya FIR Gate size ki ya FIR process ke parameter mein koi problem Hogi ya ring plazer mein problem Hogi ya temperature ki problem bhi hai ho sakti hai doston usko do teen bar padi hai technical post Hoti Hai Ek Bar Mein samajh mein nahin aati hai aur Is Tarah Se agar aap koi doubt ho to comment Kariye aap Hamen Mel bhi kar sakte hain aur Ab Hamari post ko share Kariye Apne doston ke sath Agar usmein Kuchh Kami Lag Rahi Hai To Hamen bataiye Ham usmein Sudhar Jarur Karenge doston aap Kuchh doubt ho to comment Mein Jarur Jarur likhiye aur Taki Ham Apne blog se aap Logon Tak pahunchkar aapki problem ko solve kar Saken aap injection molding mein kisi bhi group mein kam kar rahe hain agar aap Businessman hai aapki factory hai aapka plant hai aapka supervisor hai aap job kar rahe hain aap padhaai kar rahe hain Kuchh Bhi kar rahe hain to Humse contact Mein Jarur Rahe aur agar aap Kisi Tarah Se Hamari help chahie to Humse contact Karen thank u

Comments

Popular posts from this blog

Types of plastic

Plastic 2 prakar ke hote hai 1 thermoplastic 2 thermosetting plastic Wo plastic jo ek baar heat dene k baad   soft ho jate hai aur easily doosrey article me convert ho jate hai .isme na unki physical property change hoti hai n chemical property change hoti bus sirf physical look change ho jata hai Jabki thermosetting plastic me  agar ek baar kisi article ko heat kiya to fir se wo dobara nhi change nhi hoga aur material degrade ho jaega aur dirty si smell aane lagti hai for example aap cooker k utensil hi lelo .isliye thermoplastics achche hote hai kyuki wo recyclable hote hai . Unse koi bahut jyada environment ka khatra bhi nhi hai . #injection molding #plastic #indiaplast #ezyplast #whatisplastic #typesofplastic #plastasia #polymer

Scale callibration

 Good evening doston aur aaj ki is post Mein Main aapko scale caliberation ke bare mein bataunga scale calibration kya hoti hai jaise ki word Se Lag Raha Haicalibration  yani calibrate karna calibrate Ham Kis chij Ko karte hain use chij ko Karte Hain Jo ki Apne pahle ki avastha se bahar a chuki hai ya FIR kharab ho chuki hai to scale ka calibration Karne Wale scale Jab kharab ho jaaye ya is Khel ki jo value Hai vah disturb Ho Jaaye Kaun the scale transducer ki baat ho rahi hai yahan per to transport ki value Jab change Ho Jaati Hai To Ham use kya karte hain fir se set Karke original value Tak Lekar Aate Hain To LV DT jo hoti hai machine Mein Char Jagah per hoti hain injection unit mein yah scale main yah scale through ke movement ke liye use Hoti Hai screw ke bad FIR clamping unit mein movement ke liye kiske use Hoti Hai clamp u ke movement ke liye use hoti hai aur ek Dai Hai adjusting ke liye ek plate use Hoti Hai is tarike se Char scale jo hai vah Hoti Hai scale ko calibrate...

What is suck back in injection molding

 Good morning dosto Suck back , Naam se hi lag rha hai ki koi cheez suck ho rhi hai yani kheechi ja rhi hai . Suck back ka matlab hua peeche ki taraf kheechna  .  Actually jab plastic melt material mold me inject ho jata hai aur injection ke baad holding  complete ho jati hai tab part cooling zone me jata hai aur isi waqt refilling bhi sath sath hoti rhti hai refilling poori hone k baad screw straight direction me back hota hai utne mm jitna set kiya jata hai. Alag alag material k liye alag alag value me set krte hai suck back  Suck back dene se drooling ki problem ko solve kiya jata hai aur sath hi sath   silver bhi troubleshoot hota hai .suck back dene se material me threading generate nhi hoti hai nozzle se