Skip to main content

Injection molding defect 6~jetting

 Aaj ke is post Mein Ham Baat Karne Wale Hain jetting problem ki actually yah problem flow se related Hai Jab plastic melt material ka flow divert ho jata hai aur ek proper tarike se nahin hota hai material mold ke andar inject tab chatting Jaisi problem Aati Hai yah problem tab Aati Hai Jab plastic surface per floor divert hota hai tab Aati Hai Kyon Aati Hai Kyunki injection speed ya FIR injection pressure bahut hi kam set Kiya gaya hai ya FIR bahut jyada set kar diya Gaya Hai To Jiski vajah se jo material ka flow Hai vah Ek Sahi tarike se nahin Ho Pa raha hai isliye proper injection pressure ko set kar dena chahie Agla point hai isliye mold ko maintain karne ke liye Sahi Temperature per M Ti Si ka upyog kar sakte hain Agar part mein koi problem a rahi hai chatting Jaisi to aap MPC ka use kar sakte hain next Hai gold ka Gate section proper size ka Nahin Hai Jiski vajah se chatting problem a rahi hai problem Aati Hai nosal ka Dayan bahut kam hai ise Sahi Karen saaf karen to nosal ka diameter jo hai vah ho sakta hai mold Ke Jo hole hai uska jo hole hai usse bahut kam ho jisse ki metal proper tarike se usmein nahin Ja Pa raha hai to use Hamen thoda karna hoga aur saaf karna hoga Sahi karna hoga Agla point HRTC ke bare mein HRTC ka HRTC hot runner temperature controller ka temperature kam hai material per nirbhar karta hai ki Kitna temperature Hamen set karna chahie aap Logon Ko honi chahie ki kis material ke liye Kitna temperature karna hai aur use hisab se HRTC ka temperature aap set kar dijiye Agla Hai Nobel ka temperature aur barrel ka temperature kam hone se chatting problem Aati Hai To nosal ke temperature ko thoda sa incres kar dijiye barrel ke temperature ko increase kar dijiye jisse ki jaise ki aap logon ne dekha ki jeet ki balancing group foodpanda ghar par hai temperature jaipur logic temperature temperature htc temperature bhoomika temperature in temperature apps lock diameter jo ki nosal Ka Hota Hai Jahan se metal flow Karta Hai inter karta hai usko bhi thoda sa satik Rakhna chahie Sahi Rakhna chahie Gate size ko Sahi Rakhna chahie injection speed injection pressure ko bhi bahut sahi Rakhna chahie bahut Kam Nahin Rakhna chahie yah Kuchh point the chatting problem Jinse solve ho sakti Hai Doston ine problems ko solve karne ke liye aapko karna kya hoga doston Yahi Kuchh parameter Bataye gaye hain Aage ke block Mein Ham aur hi jyada point Lekar Ke Aane Wale Hain Doston jismein Ki Ham Karenge Uske bare mein baat karenge filhal ke liye aap Hamari block ko Hamare post ko like kar dijiye Agar aapke man mein koi doubt ho aap injection molding plant Mein kam kar rahe hain aapko manpower jarurat hai to Humse kar sakte hain doston aur Agar Kisi bhi Tarah ki koi bhi problem a rahi hai plus social media ke har platform per available hai dhanyvad

Comments

Popular posts from this blog

What is suck back in injection molding

 Good morning dosto Suck back , Naam se hi lag rha hai ki koi cheez suck ho rhi hai yani kheechi ja rhi hai . Suck back ka matlab hua peeche ki taraf kheechna  .  Actually jab plastic melt material mold me inject ho jata hai aur injection ke baad holding  complete ho jati hai tab part cooling zone me jata hai aur isi waqt refilling bhi sath sath hoti rhti hai refilling poori hone k baad screw straight direction me back hota hai utne mm jitna set kiya jata hai. Alag alag material k liye alag alag value me set krte hai suck back  Suck back dene se drooling ki problem ko solve kiya jata hai aur sath hi sath   silver bhi troubleshoot hota hai .suck back dene se material me threading generate nhi hoti hai nozzle se  

Types of plastic

Plastic 2 prakar ke hote hai 1 thermoplastic 2 thermosetting plastic Wo plastic jo ek baar heat dene k baad   soft ho jate hai aur easily doosrey article me convert ho jate hai .isme na unki physical property change hoti hai n chemical property change hoti bus sirf physical look change ho jata hai Jabki thermosetting plastic me  agar ek baar kisi article ko heat kiya to fir se wo dobara nhi change nhi hoga aur material degrade ho jaega aur dirty si smell aane lagti hai for example aap cooker k utensil hi lelo .isliye thermoplastics achche hote hai kyuki wo recyclable hote hai . Unse koi bahut jyada environment ka khatra bhi nhi hai . #injection molding #plastic #indiaplast #ezyplast #whatisplastic #typesofplastic #plastasia #polymer

What is l/d ratio

L/d ratio👉 Yah screw ki flight length aur outside diameter Ka anupat Hota Hai jyadatar yah anupat 20:1 hota hai aur ya 18:1 se 24 * 1 Tak hota hai dharmon set material Mein yah anupat 12:1 se 16 is Tu Van tak rahata hai Jyada Se Jyada share hit generate Hoti Hai plastic Mein Bina Jale Hue Jitna Jyada mixing hoti hai utna hi h*** genus melt hota hai Jitna Jyada residence time hota hai plastic ka barrel mein aur LCM Jyada hoga to kam cycle time mein Bade shots nikal Lete Hain. To yah To Kuchh definition Thi doston ab main aapko Aasan bhasha mein samjhata hun ki l y Di ratio Hota kya hai dekhiae jo screw ki lambai hoti hai usko Ham bolate Hain flight length theek Hai Doston Kyunki yah flight Jahan se start hoti hai aur jahan tak flight ka end hota hai rinklanjar wale part Ko Chhod Karke is group mein vah lambai kahlati hai flight length aur jo nominal diameter hota hai is group ka usko Ham outside Tak napte Hain usko Ham bolate Hain out side diameter ine donon ka hi jo ratio Hota Hai vah...