Cycle time in injection molding process

Hii.... Friends
Aaj. Ki post me main aapse cycle time ke bare me breifly discuss karna chahta hoo  par isse pahle agar post me likhte waqt koi spelling mistake ho to uske liye  Sorry dost main sudhar jaroor karunga

Molded part ko banaane me bahut sare process hote hai jinko complete hone me kuch time lagtaa hai yahi sara time ek cycle create karta hai jisse cycle time banta hai jaise sabse pahle mold band hota hai 
Fir injection unit forward hoti hai uske baad injection hota hai jisme plastic melt material fill hota hai mold me uske baad   material holding zone me jata hai aur waha kuch waqt k liye material hold hota hai jisse part poori tarah impression me bhar jaye bina koi defect  aaye 
Uske baad part cooling zone me aata hai cool hone k liye yaha par cooling time apply hota hai
Cool hone k sath sath refilling bhi hoti hai  agle shot ko mold me inject karne ke liye 
Fir suck back hota hai cool hone ke baad  mold open hota hai  jise mold opening time bolte hai fir set kiye hue position par pahuch kar  ejector position  aage aati hai part ko eject karne k liye  jisse ejector forward time bolte hai aur uske baad fir se start hota hai mold closing time .
Ti is tarah se jo formula banta hai cooling time ka wo neeche diya gya hai
Cycle time = mold closing time+injection time+holding time+cooling time+mold opening time+ ejector forward time .



Iske matlab hua ki poore process me yahi steps baar baar ho rahi hai aur baar baar part ban rha hai jisme kuch waqt lag rha hai jisse ek cyclic order create ho rha hai .
Part banane me ek process ko complete hone me jo waqt lag rha hai wagi uska cycle time kahlata hai .


Therefore the total time taken to complete one cycle in manufacturing a plastic molded part id called cycle time. 
Aaj. Ki is post ko yahi rokte hai aur milte hai kal ek nayi post k sath .
Jai hind hai bharat.
 


Comments

Popular posts from this blog

Types of plastic

Plastic 2 prakar ke hote hai 1 thermoplastic 2 thermosetting plastic Wo plastic jo ek baar heat dene k baad   soft ho jate hai aur easily doosrey article me convert ho jate hai .isme na unki physical property change hoti hai n chemical property change hoti bus sirf physical look change ho jata hai Jabki thermosetting plastic me  agar ek baar kisi article ko heat kiya to fir se wo dobara nhi change nhi hoga aur material degrade ho jaega aur dirty si smell aane lagti hai for example aap cooker k utensil hi lelo .isliye thermoplastics achche hote hai kyuki wo recyclable hote hai . Unse koi bahut jyada environment ka khatra bhi nhi hai . #injection molding #plastic #indiaplast #ezyplast #whatisplastic #typesofplastic #plastasia #polymer

Scale callibration

 Good evening doston aur aaj ki is post Mein Main aapko scale caliberation ke bare mein bataunga scale calibration kya hoti hai jaise ki word Se Lag Raha Haicalibration  yani calibrate karna calibrate Ham Kis chij Ko karte hain use chij ko Karte Hain Jo ki Apne pahle ki avastha se bahar a chuki hai ya FIR kharab ho chuki hai to scale ka calibration Karne Wale scale Jab kharab ho jaaye ya is Khel ki jo value Hai vah disturb Ho Jaaye Kaun the scale transducer ki baat ho rahi hai yahan per to transport ki value Jab change Ho Jaati Hai To Ham use kya karte hain fir se set Karke original value Tak Lekar Aate Hain To LV DT jo hoti hai machine Mein Char Jagah per hoti hain injection unit mein yah scale main yah scale through ke movement ke liye use Hoti Hai screw ke bad FIR clamping unit mein movement ke liye kiske use Hoti Hai clamp u ke movement ke liye use hoti hai aur ek Dai Hai adjusting ke liye ek plate use Hoti Hai is tarike se Char scale jo hai vah Hoti Hai scale ko calibrate...

What is suck back in injection molding

 Good morning dosto Suck back , Naam se hi lag rha hai ki koi cheez suck ho rhi hai yani kheechi ja rhi hai . Suck back ka matlab hua peeche ki taraf kheechna  .  Actually jab plastic melt material mold me inject ho jata hai aur injection ke baad holding  complete ho jati hai tab part cooling zone me jata hai aur isi waqt refilling bhi sath sath hoti rhti hai refilling poori hone k baad screw straight direction me back hota hai utne mm jitna set kiya jata hai. Alag alag material k liye alag alag value me set krte hai suck back  Suck back dene se drooling ki problem ko solve kiya jata hai aur sath hi sath   silver bhi troubleshoot hota hai .suck back dene se material me threading generate nhi hoti hai nozzle se